It is the distance between the external surface and the point on which Vickers hardness assumes the conventional value of HV = 685 (HRC ~ 59).It is determined as per point 2.1.1
The hardened surface may be approximately evaluated, with the help of a centisimal comparator with 20 magnification, considering the area (on a transversal section of the piece) including the external surface and the point on which the coloring of the surface etched by the reactive agent, change from blue to brown - yellow.
The section of the piece is polished and etched with reactive agent Nital 4% for about 30 seconds。

签到天数: 96 天

[LV.6]常住居民II

发表于 2012-2-18 11:06:29 | 显示全部楼层
It is the distance between the external surface and the point on which Vickers hardness assumes the conventional value of HV = 685 (HRC ~ 59).
这是从表面处到传统意义上假设的维氏硬度值为685(HRC-59)测定点的距离。
It is determined as per point 2.1.1
这是每个点被确定的方法。
The hardened surface may be approximately evaluated,with the help of a centisimal comparator with 20 magnification,considering the area (on a transversal section of the piece) including the external surface and the point on which the coloring of the surface etched by the reactive agent, change from blue to brown - yellow.
在20倍比较仪器的帮助下,被硬化的表面可以粗略的计算,考虑的区域(在一个横截面上)包括外表面和这个点,在活性剂的酸蚀下,从表面到这个点的颜色从蓝色变为棕黄色。
The section of the piece is polished and etched with reactive agent Nital 4% for about 30 seconds。
切割件抛光后用4%的硝酸酒精溶液腐蚀30秒。
水平有限,仅供参考!
回复 顶 踩

使用道具 举报

您需要登录后才可以回帖 登录 | 立即注册

本版积分规则

QQ|Archiver|手机版|小黑屋|热处理论坛 ( 苏ICP备2021037530号|苏公网安备32059002001695号 )
Copyright © 2005-2026, rclbbs.com 苏州热协网络技术有限公司 版权所有

GMT+8, 2026-10-27 09:24 , Processed in 0.030510 second(s), 25 queries .

Powered by Discuz! X3.5

© 2001-2026 Discuz! Team.

快速回复 返回顶部 返回列表