[分享] Fatigue of Structures Materials

[复制链接]

该用户从未签到

发表于 2009-10-21 10:34:52 | 显示全部楼层 |阅读模式
北京中仪天信科技有限公司
英文pdf原版,清晰,搜索论坛未发现重复。
欢迎大家下载。
About the contents of the book

The book starts with chapters on basic issues:
• Fatigue as a phenomenon occurring in the material (Chapter 2).
• Because stress concentrations in a structure are of paramount importance for fatigue, stress distributions around notches and stress concentration factors (Kt ) are discussed in Chapter 3.
• Residual stresses can have a significant effect on fatigue. A special chapter is presented on these stresses (Chapter 4).
• After fatigue cracks have been nucleated, the stress intensity factor (K) is a controlling parameter for the severity of the stress distribution around the crack tip and fatigue crack growth. The concept of the stress intensity factor is discussed in Chapter 5.
• Fatigue properties, including the fatigue limit, S-N curves, fatigue diagrams, and also fatigue crack growth are discussed in Chapters 6 to 8. Some prediction problems are discussed in these chapters. 本帖最后由 wangqinghua196 于 2009-10-31 20:38 编辑

Fatigue of Structures and Materials.rar

40.36 MB, 下载次数: 1304

评分

参与人数 1热处理币 +20 收起 理由
wangqinghua196 + 20 精品资料!

查看全部评分

您需要登录后才可以回帖 登录 | 立即注册

本版积分规则

QQ|Archiver|手机版|小黑屋|热处理论坛 ( 苏ICP备2021037530号|苏公网安备32059002001695号 )
Copyright © 2005-2026, rclbbs.com 苏州热协网络技术有限公司 版权所有

GMT+8, 2026-10-29 09:29 , Processed in 0.023875 second(s), 25 queries .

Powered by Discuz! X3.5

© 2001-2026 Discuz! Team.

快速回复 返回顶部 返回列表