[书籍] 《Solid State Transformation And Heat Treatment》Alain Hazotte.2005

[复制链接]

签到天数: 3047 天

[LV.Master]伴坛终老

发表于 2022-6-3 15:32:09 | 显示全部楼层 |阅读模式
北京中仪天信科技有限公司
固态转变和热处理
0.jpg
The final microstructures of engineering materials are very often obtained through solid state
transformation process(es). A good knowledge of the basic transformation mechanisms, associated with a tight control of the relevant process parameters, are vital to optimise the material
properties. Thus, one symposium of Euromat 2003, the 8th European Congress and Exhibition
on Advanced Materials and Processes held in Lausanne (CH) on 1-5 september 2003, was logically devoted to “Solid State Transformations and Heat Treatments”. This symposium was open
to experimental and/or modelling works increasing this knowledge or/and explicitly making use
of it for process/property optimisation. About sixty oral and poster contributions were given.
Both diffusion-controlled and diffusionless transformations were concerned, covering a large
range of metallic or non metallic materials. The sessions gave rise to rich and animated debates
and drew the major directions of future development, specially in the field of transformation
modelling.

《Solid State Transformation And Heat Treatment》Alain Hazotte.2005.pdf

4.98 MB, 下载次数: 126

签到天数: 252 天

[LV.8]以坛为家I

发表于 2022-7-1 08:41:56 | 显示全部楼层
多看看国外文献长长见识,就是外文的看着累人,几个月能看完就不错了:lol
回复 顶 踩

使用道具 举报

您需要登录后才可以回帖 登录 | 立即注册

本版积分规则

QQ|Archiver|手机版|小黑屋|热处理论坛 ( 苏ICP备2021037530号|苏公网安备32059002001695号 )
Copyright © 2005-2026, rclbbs.com 苏州热协网络技术有限公司 版权所有

GMT+8, 2026-10-27 10:19 , Processed in 0.023914 second(s), 24 queries .

Powered by Discuz! X3.5

© 2001-2026 Discuz! Team.

快速回复 返回顶部 返回列表