[书籍] 《Heat treatment : master control manual》William E.Bryson.2015

[复制链接]

签到天数: 3047 天

[LV.Master]伴坛终老

发表于 2022-6-3 14:35:20 | 显示全部楼层 |阅读模式
北京中仪天信科技有限公司
热处理:主控手册
1.jpg
This indispensable manual focuses on heat-treating by ASM, SME, and AISI standards. It has been created for use in student education, as well as to guide professionals who have been heat treating their entire lives. Written without the typical metallurgical jargon, it will serve as a training manual from day one in learning how to heat treat a metal, and then also serve as a day-to-day reference for a lifetime. This manual zeros in on the popular tool steels, alloy steels, heat-treatable stainless steels, case hardening steels, and more. It deals with these metals with up-to-date usage and processing recipes. What is different with this manual from all the others is that it doesnt just deal with the heat-treatment process, it also covers the continuation of the hardening process with cryogenics. It is written to help those who may want a thorough understanding of what goes on in the process of heat-treating and how to do it better. It also shows how proper heat and cryogenic processing can save your company money through longer life tooling, decarb-free and stress relief, all while learning how to create a better, finer grain structure. This manual shows that hardness is only an indication of hardness, and that the real money savings is in the fine grained structure. Written for toolmakers, engineers, heat-treaters, procurement, management personnel, and anyone else who is involved in metals, this manual covers the complete range of thermally treated metals from 2400°F down to 320°F

《Heat Treatment:Master Control Manual》William E.Bryson.2015.pdf

19.72 MB, 下载次数: 513

签到天数: 252 天

[LV.8]以坛为家I

发表于 2022-7-1 08:40:23 | 显示全部楼层
没明白啥叫主控手册?
下面的简介百度翻译了一下,好像是本很实用的书:
本不可或缺的手册重点介绍了ASM、SME和AISI标准的热处理。它被创建用于学生教育,也用于指导终身从事热处理的专业人士。它没有典型的冶金术语,从学习如何热处理金属的第一天起就是一本培训手册,然后终身作为日常参考。本手册介绍了常用的工具钢、合金钢、可热处理不锈钢、表面硬化钢等。它以最新的使用和加工配方处理这些金属。与所有其他手册不同的是,本手册不仅涉及热处理过程,还涵盖了低温硬化过程的延续。本书旨在帮助那些希望彻底了解热处理过程中发生的事情以及如何更好地进行热处理的人。它还展示了适当的加热和低温处理如何通过使用寿命更长的模具、无脱碳和消除应力来节省公司资金,同时学习如何创建更好、更细的晶粒结构。本手册表明,硬度只是硬度的一个指标,而真正节省资金的是细粒度结构。本手册适用于工具制造商、工程师、热处理人员、采购、管理人员和任何其他金属相关人员,涵盖了从2400°F到320°F的热处理金属的完整范围
回复 顶 踩

使用道具 举报

您需要登录后才可以回帖 登录 | 立即注册

本版积分规则

QQ|Archiver|手机版|小黑屋|热处理论坛 ( 苏ICP备2021037530号|苏公网安备32059002001695号 )
Copyright © 2005-2026, rclbbs.com 苏州热协网络技术有限公司 版权所有

GMT+8, 2026-10-28 00:19 , Processed in 0.024560 second(s), 24 queries .

Powered by Discuz! X3.5

© 2001-2026 Discuz! Team.

快速回复 返回顶部 返回列表