Effect of intrinsic heat treatment on the precipitate formation of X40CrMoV5...

[复制链接]

签到天数: 904 天

[LV.10]以坛为家III

发表于 2025-3-24 22:35:19 | 显示全部楼层 |阅读模式
北京中仪天信科技有限公司
【作  者】Antonio Carlos de F. Silveira , Lisa T. Belkacemi Pedro José de Castro
【刊  名】 Acta Materialia
【关键词】Additive manufacturingIntrinsic heat treatmentTool steelCarbide precipitationHigh energy synchrotron X-ray diffractionAtom probe tomography
【摘 要】Additively manufactured components are generally heat treated to remove the undesired microstructure formed during the repeated heating-cooling cycles inherent to the process, known as intrinsic heat treatment (IHT). Recently, the IHT has been explored as a driving force for precipitation hardening in steels which can potentially shorten the manufacturing chain of AM components. However, the mechanisms behind the formation of secondary phase precipitates during the complex thermal history remains unclear. In this work, a combination of in situ high energy X-ray diffraction, atom probe tomography, scanning and transmission electron microscopy were used to reveal the precipitation sequence in an X40CrMoV5–1 tool steel during laser-directed energy deposition (L-DED). V-rich MCN and V8CN7 carbonitrides, as well as, Fe-Cr-rich M3C and M7C3 carbides were formed at different stages of the L-DED. Their evolution and resulting chemical stoichiometry was correlated to the exact phase transformation occurring in the microstructure during the IHT over different regions along the built direction. Finally, the combined results from the in situ and ex situ experiments enabled us to retrace the history of the full microstructure during the L-DED process. The findings lead to the conclusion that secondary hardening effect in tool steel is, as expected, sensitive to the severity of the IHT, and if limited, can result in a tempered microstructure comparable to the ones conventionally obtained after tempering heat treatments.

Effect of intrinsic heat treatment on the precipitate formation of.pdf

27.33 MB, 下载次数: 59

您需要登录后才可以回帖 登录 | 立即注册

本版积分规则

QQ|Archiver|手机版|小黑屋|热处理论坛 ( 苏ICP备2021037530号|苏公网安备32059002001695号 )
Copyright © 2005-2026, rclbbs.com 苏州热协网络技术有限公司 版权所有

GMT+8, 2026-10-27 11:10 , Processed in 0.023944 second(s), 25 queries .

Powered by Discuz! X3.5

© 2001-2026 Discuz! Team.

快速回复 返回顶部 返回列表