[Translation] alpha case

[复制链接]

该用户从未签到

发表于 2010-6-10 20:39:00 | 显示全部楼层 |阅读模式
北京中仪天信科技有限公司
What is the meaning of "alpha case"?(Alpha Case: Wrought Titanium)

签到天数: 2 天

[LV.1]初来乍到

发表于 2010-6-10 22:17:46 | 显示全部楼层
From Wikipedia
In metallurgy, alpha case is the oxygen-enriched phase that occurs when titanium and its alloys are exposed to heated air or oxygen. Alpha case is brittle, and tends to create a series of microcracks which will reduce the metal's performance and it's fatigue properties. Alpha case can be avoided by processing in a vacuumed environment, but, due to its costs it is usually eliminated via machining or chemical milling

评分

参与人数 1热处理币 +2 收起 理由
bill_bush + 2 感谢支持!

查看全部评分

回复 顶 踩

使用道具 举报

该用户从未签到

 楼主| 发表于 2010-6-30 21:29:44 | 显示全部楼层
Thank you!
回复 顶 踩

使用道具 举报

该用户从未签到

 楼主| 发表于 2010-6-30 21:33:05 | 显示全部楼层
洛氏硬度的ASTM测试标准,供大家参考!

ASTM E18-03 Rockwell Hardness.pdf

304.88 KB, 下载次数: 71

回复 顶 踩

使用道具 举报

您需要登录后才可以回帖 登录 | 立即注册

本版积分规则

QQ|Archiver|手机版|小黑屋|热处理论坛 ( 苏ICP备2021037530号|苏公网安备32059002001695号 )
Copyright © 2005-2026, rclbbs.com 苏州热协网络技术有限公司 版权所有

GMT+8, 2026-10-28 15:32 , Processed in 0.025005 second(s), 25 queries .

Powered by Discuz! X3.5

© 2001-2026 Discuz! Team.

快速回复 返回顶部 返回列表