Vacuum heat treatment and high pressure gas quenching(《真空热处理及高压气淬》)

By Jean Jaques Since, Olaf Irretier

This technical article reviews high pressure gas quenching technique
using different quenching processes for improvement of part quality, cost
and mechanical properties.
Gas quenching represents an environmental friendly alternative to commonly
used atmospheric oil quenching. ECM has developed innovative
quenching processes for quality and performance improvement on
finished parts in the automotive and gear industry. The goal is to reduce
the level of distortion as well as the increase of mechanical properties.
Industrial applications will be shown with detailed data. Explanations will
be given on improvements and manufacturing process cost savings.
These processes could be directly applied to existing processes for global
cost reduction and quality improvement or for future products which
need increased performance and higher levels of quality.



Vacuum heat treatment and high pressure gas quenching.jpg

Vacuum heat treatment and high pressure gas quenching.pdf

582.47 KB, 下载次数: 37

您需要登录后才可以回帖 登录 | 立即注册

本版积分规则

QQ|Archiver|手机版|小黑屋|热处理论坛 ( 苏ICP备2021037530号|苏公网安备32059002001695号 )
Copyright © 2005-2026, rclbbs.com 苏州热协网络技术有限公司 版权所有

GMT+8, 2026-10-26 13:04 , Processed in 0.024709 second(s), 25 queries .

Powered by Discuz! X3.5

© 2001-2026 Discuz! Team.

快速回复 返回顶部 返回列表