国外二手设备网站看到的设备,附介绍

Model:                                                             VMH-T-363648
Work Chamber:                                               36” High x 36” Wide x 48” Long (Full
                                                                        Round Hot Zone)
Insulation:                                                         4” High-Purity Ceramic Fiber, (currently oily so may

                                                                        want to clean and reline with new Kaowool)
Heating Elements:                                             Wound Chromel-Alumel Wire Type
Floor Space:                                                     120” H x 191” W x 160” L
Temperature:                                                    Uniformity:  ±15°F *    (Last survey was +/- 4°F)
Work Loading:                                                 3,000 lb. OEM Rating
Operating                                                         Temperature 1450°F Maximum
Power Requirements:                                        120 KVA, Heating (480/3/60 input)
Ultimate Vacuum:                                             A conditioned, clean dry empty and
                                                                        out-gassed system will pump to 100
                                                                        microns or less within 20 minutes *
Operating Vacuum:                                           During tempering the normal
                                                                        operating pressure is between 400 to
                                                                        600 torr,
Fan Assembly:                                                  10 HP motor
Compressed Air Requirements:                         Intermittent demand at 90 psig
Cooling Water:                                                 20 to 30 GPM
Nitrogen Backfill:                                              330 Cubic Feet
Vacuum Pumps:                                                Stokes 412-11 and Roots 615RGS,
                                                                        Both recently rebuilt
Controls:                                                          All new control panel including instruments,
                                                                        controllers and vacuum sensors recently,
                                                                        Honeywell HC 900 temperature controller
Overall Footprint as currently installed:              13ft D x 16ft W x 9.5ft H
Current Location:                                              Northwestern U.S.
Price:                                                                $95,000  
Terms:                                                              50% Down, Balance prior to loading
                                                                        unless otherwise agreed by owner.
F.O.B.:                                                             Current Location, As-Is  
(Removed and placed in storage July, 2007)                                                                     
*  Original OEM specs, Not guaranteed on used equipment
1.jpg
2.jpg
3.jpg
4.jpg
5.jpg
6.jpg

评分

参与人数 1热处理币 +15 收起 理由
stove + 15 感谢上传!

查看全部评分

该用户从未签到

 楼主| 发表于 2008-3-28 13:52:22 | 显示全部楼层
Item # 3278  -  40+ Bar Brew Sinterhip Vacuum Furnace:         Price Reduced May 7, 2007

Rebuilt 1987 Brew Sinterhip Vacuum Furnace, max. 1400°C, (approx. 1000°C
with retort), Stokes 212H-11 with Stokes 401 Blower (rebuilt by United Vacuum
approx.  10 operational hours ago), No diffusion pump, Ultimate Vacuum is 30 microns
(clean, dry & empty), Rated for 600 PSIG (Code Stamp says 660 PSIG) internal
pressure for HIP operation, Operating pressure range:  50 microns to 500 PSIG.  
Useable work area:  18" Dia. x 24"   Electrical:  480V/3Ph/260 kVA, 350 Amp Breaker,
Cooling water reqm't:  50 GPM at 50 PSIG and 70°F.  Chamber has been Ultrasonic
inspected for integrity.  Practically new condition, less than 100 hours estimated total

use.  
VRT Power Supply with water-cooled cables.  Bottom elements are not installed in
photos below, and retort door is not shown.    Location:  Western U.S.
Price:  $125,000   Offers considered
1.jpg
2.jpg
3.jpg
4.jpg
5.jpg
回复 顶 踩

使用道具 举报

该用户从未签到

 楼主| 发表于 2008-3-28 13:56:10 | 显示全部楼层
Item # 3304:  6-Bar Vacuum Heat Treating Furnace:

1996 Vac Aero, 6-Bar Pressure Quench Vacuum Heat Treating Furnace,
Model # VAH 4848 MP6, Work Zone:  36"W x 48"D x 30"H, (Alternate load size
by raising hearth:  48"W x 48"L x 22"H), 2400°F, 200 HP 10,000 CFM External
Cooling Blower, 480V/3Phase/60Hz, 285kVA, Hunterdon VRT Power Supply,
2,000,000 BTU/hr Gas Cool Heat Exchanger, Load Rating:  2500 lb. at 2400°F,
Vacuum Pumps:  Stokes 412-11 with Roots 615RGS Blower, Honeywell S9000
Temperature Controller with UDC3000 Hi-Limit, Edwards AGC Vacuum Control.
Currently still installed, but will be removed for storage later in December.  Removal
costs will be added to price.  Includes water cooling system and Loader
Price:  $295,000    Location:  Midwestern U.S.
4976.jpg
回复 顶 踩

使用道具 举报

该用户从未签到

 楼主| 发表于 2008-3-28 13:59:55 | 显示全部楼层
Item # 3267  -  36"W x 48"D x 36"H  C.I. Hayes Vacuum Temper:        

Model:                                                             VMH-T-363648
Work Chamber:                                               36” High x 36” Wide x 48” Long (Full
                                                                        Round Hot Zone)
Insulation:                                                         4” High-Purity Ceramic Fiber, (currently oily so may

                                                                        want to clean and reline with new Kaowool)
Heating Elements:                                             Wound Chromel-Alumel Wire Type
Floor Space:                                                     120” H x 191” W x 160” L
Temperature:                                                    Uniformity:  ±15°F *    (Last survey was +/- 4°F)
Work Loading:                                                 3,000 lb. OEM Rating
Operating                                                         Temperature 1450°F Maximum
Power Requirements:                                        120 KVA, Heating (480/3/60 input)
Ultimate Vacuum:                                             A conditioned, clean dry empty and
                                                                        out-gassed system will pump to 100
                                                                        microns or less within 20 minutes *
Operating Vacuum:                                           During tempering the normal
                                                                        operating pressure is between 400 to
                                                                        600 torr,
Fan Assembly:                                                  10 HP motor
Compressed Air Requirements:                         Intermittent demand at 90 psig
Cooling Water:                                                 20 to 30 GPM
Nitrogen Backfill:                                              330 Cubic Feet
Vacuum Pumps:                                                Stokes 412-11 and Roots 615RGS,
                                                                        Both recently rebuilt
Controls:                                                          All new control panel including instruments,
                                                                        controllers and vacuum sensors recently,
                                                                        Honeywell HC 900 temperature controller
Overall Footprint as currently installed:              13ft D x 16ft W x 9.5ft H
Current Location:                                              Northwestern U.S.
Price:                                                                $95,000  
Terms:                                                              50% Down, Balance prior to loading
                                                                        unless otherwise agreed by owner.
F.O.B.:                                                             Current Location, As-Is  
(Removed and placed in storage July, 2007)                                                                     
*  Original OEM specs, Not guaranteed on used equipment
1.jpg
2.jpg
3.jpg
4.jpg
5.jpg
回复 顶 踩

使用道具 举报

该用户从未签到

 楼主| 发表于 2008-3-28 14:01:25 | 显示全部楼层
Item # 3233 (VF-150)  -  Vacuum Deoiler:

Purchased New in 1993. Model HR 50x48DG. Nominal Work Zone: 36" x 30"H x 48"D.
Max. Load & Temperature: 3000lbs @ 650°F. Operating Temp: 250-650°F +/-10°F.
Cleanup Temp: 800°F (Max. 2 hours). Roughing Pump: 400/300 CFM.
Partial Pressure: Nitrogen. Gas Cooling: 50 HP Motor, external. Backfill Gas: Nitrogen.  
Programmer: Honeywell DCP-200(single channel). Overtemperature Instrument:
Honeywell UDC-2000. Vacuum Instrument: Leybold Inficon PG-3.
Asking Price: $80,000
P5010422.jpg
P5010423.jpg
回复 顶 踩

使用道具 举报

该用户从未签到

 楼主| 发表于 2008-3-28 14:03:02 | 显示全部楼层
Item # 3200, VF144  -  C.I. Hayes Vacuum Carburizing/Oil Quench Furnace:

C.I. Hayes Vacuum Carburizing/Oil Quench Furnace with updated Honeywell control system.
Working dimensions are 48" deep, 30" wide by 32" high. Equipped with an automated vacuum
carburizing system. The furnace includes two load carts and a wash system. Furnace is in good
operating condition and was in use until very recently.
Asking Price: $99,000CDN     Approx. $82,500 U.S. Dollars
1.jpg
2.jpg
回复 顶 踩

使用道具 举报

该用户从未签到

 楼主| 发表于 2008-3-28 14:07:11 | 显示全部楼层
Item # 3109:  Factory Reconditioned and New Loaders / Unloaders:
3,000 lb. Capacity Loaders, Factory Reconditioned and New, Then Customized to Your Vacuum Furnace,
Polyurethane Wheels, Heavy Duty Guide Shafts, Self-Propelled or Manual, Hydraulic Lift, with
Integral Battery Charger.  Other Sizes Also Available.
BJ_Front_with_Parts.jpg
BJ_Part_from_Side.jpg
BJ_Parts_into_Furnace.jpg
回复 顶 踩

使用道具 举报

您需要登录后才可以回帖 登录 | 立即注册

本版积分规则

QQ|Archiver|手机版|小黑屋|热处理论坛 ( 苏ICP备2021037530号|苏公网安备32059002001695号 )
Copyright © 2005-2026, rclbbs.com 苏州热协网络技术有限公司 版权所有

GMT+8, 2026-10-28 11:31 , Processed in 0.029715 second(s), 28 queries .

Powered by Discuz! X3.5

© 2001-2026 Discuz! Team.

快速回复 返回顶部 返回列表