[Help] 块状铁素体对应的专业英语词汇是?

[复制链接]

签到天数: 299 天

[LV.8]以坛为家I

发表于 2013-4-25 15:49:04 | 显示全部楼层 |阅读模式
北京中仪天信科技有限公司
just as show in the title,please help me.

签到天数: 299 天

[LV.8]以坛为家I

 楼主| 发表于 2013-4-25 15:49:33 | 显示全部楼层
also 条状铁素体
回复 顶 踩

使用道具 举报

该用户从未签到

发表于 2013-4-25 16:58:52 | 显示全部楼层
bulk ferrite,我猜的
回复 顶 踩

使用道具 举报

签到天数: 329 天

[LV.8]以坛为家I

发表于 2013-4-26 12:12:31 | 显示全部楼层
massive ferrite or polygonal ferrite.
回复 顶 踩

使用道具 举报

签到天数: 123 天

[LV.7]常住居民III

发表于 2013-4-26 21:50:48 | 显示全部楼层
massive ferrite   massive ferrite
回复 顶 踩

使用道具 举报

签到天数: 9 天

[LV.3]偶尔看看II

发表于 2013-4-27 13:06:45 | 显示全部楼层
blocky ferrite (刚好昨天收到老外的邮件里提到块状铁素体)

评分

参与人数 1热处理币 +5 收起 理由
我心飞翔eric + 5 感谢支持!

查看全部评分

回复 顶 踩

使用道具 举报

签到天数: 299 天

[LV.8]以坛为家I

 楼主| 发表于 2013-4-27 14:32:33 | 显示全部楼层
回复 顶 踩

使用道具 举报

签到天数: 3 天

[LV.2]偶尔看看I

发表于 2013-4-28 09:03:17 | 显示全部楼层
块状铁素体[多边形铁素体]   :granular ferrile
                            polygonal ferrile
摘自GB7232---57标准

评分

参与人数 1热处理币 +5 收起 理由
chenze2008 + 5 感谢支持!

查看全部评分

回复 顶 踩

使用道具 举报

签到天数: 299 天

[LV.8]以坛为家I

 楼主| 发表于 2013-5-2 12:49:13 | 显示全部楼层
温庆远 发表于 2013-4-28 09:03
块状铁素体[多边形铁素体]   :granular ferrile
                            polygonal ferrile
摘自GB7 ...

Thanks for helping ,Mr Wen.
回复 顶 踩

使用道具 举报

签到天数: 3 天

[LV.2]偶尔看看I

发表于 2013-5-3 12:37:54 | 显示全部楼层
举手之劳,不必客气。
回复 顶 踩

使用道具 举报

签到天数: 22 天

[LV.4]偶尔看看III

发表于 2013-5-7 09:36:56 | 显示全部楼层
Pearlite is often said to be a two-phased, lamellar (or layered) structure composed of alternating layers of alpha-ferrite and cementite that occurs in some steels and cast irons.

course%20pearlite2.jpg

Pearlite was first identified by Henry Clifton Sorby and initially named sorbite, however the similarity of microstructure to nacre and especially the optical effect caused by the scale of the structure made the alternative name more popular.

656px-H_C_Sorby_2729.jpg



回复 顶 踩

使用道具 举报

签到天数: 22 天

[LV.4]偶尔看看III

发表于 2013-5-7 09:40:43 | 显示全部楼层
The strength of pearlite is determined by the scale of ferrite and cementile.

Pearlite.jpg

回复 顶 踩

使用道具 举报

签到天数: 22 天

[LV.4]偶尔看看III

发表于 2013-5-7 09:42:38 | 显示全部楼层
Sorry,I was onfused.

Ferrite, also known as α-ferrite (α-Fe) or alpha iron, is a materials science term for pure iron, with a body-centered cubic crystal structure. It is this crystalline structure which gives steel and cast iron their magnetic properties, and is the classic example of a ferromagnetic material.[1]

It has a strength of 280 N/mm2[citation needed] and a hardness of approximately 80 Brinell.[2]

Mild steel (carbon steel with up to about 0.2 wt% C) consist mostly of ferrite, with increasing amounts of pearlite (a fine lamellar structure of ferrite and cementite) as the carbon content is increased. Since bainite (shown as ledeburite on the diagram at the bottom of this page) and pearlite each have ferrite as a component, any iron-carbon alloy will contain some amount of ferrite if it is allowed to reach equilibrium at room temperature. The exact amount of ferrite will depend on the cooling processes the iron-carbon alloy undergoes as it cools from liquid state.

In pure iron, ferrite is stable below 910 °C (1,670 °F). Above this temperature the face-centred cubic form of iron, austenite (gamma-iron) is stable. Above 1,390 °C (2,530 °F), up to the melting point at 1,539 °C (2,802 °F), the body-centred cubic crystal structure is again the more stable form of delta-ferrite (δ-Fe). Ferrite above the critical temperature A2 (Curie temperature) of 771 °C (1,044 K; 1,420 °F), where it is paramagnetic rather than ferromagnetic, is beta ferrite or beta iron (β-Fe). The term beta iron is seldom used because it is crystallographically identical to, and its phase field contiguous with, α-Fe.

Only a very small amount of carbon can be dissolved in ferrite; the maximum solubility is about 0.02 wt% at 723 °C (1,333 °F) and 0.005% carbon at 0 °C (32 °F).[3] This is because carbon dissolves in iron interstitially, with the carbon atoms being about twice the diameter of the interstitial "holes", so that each carbon atom is surrounded by a strong local strain field. Hence the enthalpy of mixing is positive (unfavourable), but the contribution of entropy to the free energy of solution stabilises the structure for low carbon content. 723 °C (1,333 °F) also is the minimum temperature at which iron-carbon austenite (0.8 wt% C) is stable; at this temperature there is a eutectoid reaction between ferrite, austenite and cementite.
回复 顶 踩

使用道具 举报

签到天数: 1660 天

[LV.Master]伴坛终老

发表于 2016-2-2 14:06:16 | 显示全部楼层
Blocky ferrite
回复 顶 踩

使用道具 举报

签到天数: 1132 天

[LV.10]以坛为家III

发表于 2023-8-21 16:45:19 来自手机 | 显示全部楼层
massive ferrite   massive ferrite
回复 顶 踩

使用道具 举报

签到天数: 125 天

[LV.7]常住居民III

发表于 2023-9-11 08:01:55 来自手机 | 显示全部楼层
块状铁素体,翻译应该是massive ferrite
回复 顶 踩

使用道具 举报

签到天数: 1132 天

[LV.10]以坛为家III

发表于 2023-9-11 08:14:05 来自手机 | 显示全部楼层
Bulk ferrite应该是这么翻译
回复 顶 踩

使用道具 举报

签到天数: 1132 天

[LV.10]以坛为家III

发表于 2023-9-18 18:30:34 来自手机 | 显示全部楼层
bulk ferrite,块状铁素体
回复 顶 踩

使用道具 举报

您需要登录后才可以回帖 登录 | 立即注册

本版积分规则

QQ|Archiver|手机版|小黑屋|热处理论坛 ( 苏ICP备2021037530号|苏公网安备32059002001695号 )