Die steel design for additive manufacturing

[复制链接]

签到天数: 904 天

[LV.10]以坛为家III

发表于 2025-3-22 22:02:39 | 显示全部楼层 |阅读模式
北京中仪天信科技有限公司
【作  者】Florian Hengsbach a c, ulius Bürger b, Anatolii Andreiev
【刊  名】 Acta Materialia
【关键词】Additive manufacturingSelective laser meltingDie steelMaterial designCALPHAD
【摘 要】 A novel printable die steel was computationally designed and experiemtnally validated for selective laser melting (SLM), utilizing the advantages of the rapid solidification processes. During gas atomization, nanoscale TiN particles are intended to be in situ precipitated at 1790 °C, nucleating δ-ferritic grains. Additionally, the chemical composition is adjusted to stabilize a complete δ-ferritic solidification via Scheil modeling to enhance the printability of the die steel. This work further introduces the concept of the matrix die steels aiming to dissolve solidification and primary carbides during solutionizing at a targeted temperature of 1100 °C. Thus, the C-content is reduced to 1.4 mol.-% (0.3 wt.-%) compared to the benchmark H13 die steel which contains 1.85 mol.-% (0.4 wt.-%). Even though a lower C-content is used, optimizing M2C driving force during tempering enables the die steel to achieve a peak hardness of 536 HV . Lastly, a superior thermal conductivity of 40 W m-1 K-1 is predicted at 450 °C for the BCC matrix of the printable matrix die steel. The material design is based on thermo-chemical models interfaced with thermodynamic calculations as implemented in the Calculated Phase Diagram (CALPHAD) method.

Die steel design for additive manufacturing.pdf

36.23 MB, 下载次数: 45

您需要登录后才可以回帖 登录 | 立即注册

本版积分规则

QQ|Archiver|手机版|小黑屋|热处理论坛 ( 苏ICP备2021037530号|苏公网安备32059002001695号 )
Copyright © 2005-2026, rclbbs.com 苏州热协网络技术有限公司 版权所有

GMT+8, 2026-10-27 14:10 , Processed in 0.024220 second(s), 25 queries .

Powered by Discuz! X3.5

© 2001-2026 Discuz! Team.

快速回复 返回顶部 返回列表