北京中仪天信科技有限公司
EPA+3015EPA+3015Ian
简介:
METHOD 3015

MICROWAVE ASSISTED ACID DIGESTION OF AQUEOUS SAMPLES AND EXTRACTS

1.0SCOPE AND APPLICATION

1.1This digestion procedure is used for the preparation of aqueous samples, mobility-procedure extracts, and wastes that contain suspended solids for analysis, by flame atomic absorption spectroscopy (FLAA), graphite furnace absorption spectroscopy (GFAA), inductively coupled argon plasma spectroscopy (ICP), or inductively coupled argon plasma mass spectrometry (ICP-MS).
The procedure is a hot acid leach for determining available metals.
Due to the rapid advances in microwave technology, consult your manufacturer's recommended instructions for guidance on their microwave digestion system and refer to the SW-846 "DISCLAIMER" when conducting analyses using Method 3015. 1.2
Samples prepared by Method 3015 using nitric acid digestion may be analyzed by FLAA, GFAA, ICP-AES, or ICP-MS for the following:


Aluminum       Lead

           Antimony          Magnesium

           Arsenic*           Manganese

            Barium             Molybdenum

   Beryllium          Nickel

         Cadmium          Potassium

        Calcium           Selenium*

      Chromium            Silver

        Cobalt                   Sodium

*Cannot be analyzed by FLAA


[ 本帖最后由 wangqinghua196 于 2009-3-15 13:40 编辑 ]

EPA+3015(英文版).pdf

209.74 KB, 下载次数: 27

您需要登录后才可以回帖 登录 | 立即注册

本版积分规则

QQ|Archiver|手机版|小黑屋|热处理论坛 ( 苏ICP备2021037530号|苏公网安备32059002001695号 )
Copyright © 2005-2026, rclbbs.com 苏州热协网络技术有限公司 版权所有

GMT+8, 2026-10-29 11:34 , Processed in 0.023921 second(s), 25 queries .

Powered by Discuz! X3.5

© 2001-2026 Discuz! Team.

快速回复 返回顶部 返回列表