[求助] 45#淬火硬度太低,急! |
| ||
| ||
| ||
| ||
|
| |
|
| |
|
| |
| ||
| ||
| ||
| ||
点评
找50号钢和40号钢相比较就可以看出结果,50号钢C 0.47-0.55,40号钢含碳量0.37-0.44
| ||
| ||