【作  者】Saurabh Kumar a, Namit N. Pai a, Sanjay Manda
【刊  名】 Acta Materialia
【关键词】Residual stress、Austenite、Martensite、Microstructure、Variant selection
【摘 要】Controlled thermomechanical processing, in the austenite phase of two different steel grades, produced 15 different martensitic microstructures. The variant selection and the hierarchy of martensite were affected. Both, hierarchy and variant selection of the predominantly lath martensite, scaled with experimental bulk martensite residual strains (α·RS). Local α·RS and martensite crystallography, on the other hand, appeared to provide an elastic strain energy minimization. A novel methodology of estimating residual strain in the ‘invisible’ austenite phase was then proposed and validated. This approach combined pixel-by-pixel prior austenite reconstruction with dynamical high-resolution Kikuchi pattern simulations. Pattern simulation-based Phantom strain(s), considering only pattern rotation, scaled linearly with experimental, micro-Laue diffraction and microtexture based, lattice strain(s). This study was then extended to a residual stress assisted, and interaction energy based, martensite variant selection model. It was clearly shown that the austenite residual stress, estimated from pattern simulations of reconstructed austenite, controlled the martensite variant selection.

Austenite residual stress and lath martensite variant selection in low carbon steels.pdf

15.74 MB, 下载次数: 44

您需要登录后才可以回帖 登录 | 立即注册

本版积分规则

QQ|Archiver|手机版|小黑屋|热处理论坛 ( 苏ICP备2021037530号|苏公网安备32059002001695号 )
Copyright © 2005-2026, rclbbs.com 苏州热协网络技术有限公司 版权所有

GMT+8, 2026-10-26 12:23 , Processed in 0.024093 second(s), 25 queries .

Powered by Discuz! X3.5

© 2001-2026 Discuz! Team.

快速回复 返回顶部 返回列表