[求助] 急求2083的机械性能和相关资料!

[复制链接]

签到天数: 3 天

[LV.2]偶尔看看I

发表于 2008-8-16 12:23:54 | 显示全部楼层 |阅读模式
北京中仪天信科技有限公司
如题,希望有相关资料的高手,能发一份

[ 本帖最后由 stigershu 于 2008-8-16 23:21 编辑 ]

签到天数: 3 天

[LV.2]偶尔看看I

发表于 2008-9-17 14:27:14 | 显示全部楼层
2083是瑞士的一种不锈钢,用于注塑模具,如果你懂英文,可以到
www.matweb.com 查看。
Swiss Steel International THYROPLAST? 2083 Plastic Mold Steel  
Categories:  Metal; Ferrous Metal; Tool Steel; Mold Steel

Material Notes:  To manufacture plastic parts, it is necessary to have steels with a high wear resistance, good polishability and etching ability, adequate corrosion resistance, and cost efficient machining properties. Employed for this purpose, as a function of the requirements are case hardening steels, quenched and tempered steels, corrosion-resistant steels, nitriding steels and maraging steels.
Corrosion resistant, good polishability. We recommend the use of vacuum-related THYROPLAST 2083 for the highest demands on polishability.

Applications

molds for processing plastics with corrosive action
Iron content calculated as remainder

Key Words:  1.2083, AISI 420
Vendors:  No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version   Download as PDF  Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program  Add to Folder:   My Folder   

  
Mechanical Properties Metric English Comments
Hardness, Brinell <= 230 <= 230 After soft annealing
Hardness, Rockwell C 40.0 40.0 After tempering at 600°C
  51.0 51.0  HRC            After tempering at 400°C (回火温度)
  52.0 52.0    HRC          After tempering at 500°C (回火温度)
  52.0 52.0    HRC           After tempering at 300°C (回火温度)
  55.0 55.0    HRC           After tempering at 200°C (回火温度)
  56.0 56.0    HRC               after quenching (淬火后)
  56.0 56.0   HRC              After tempering at 100°C
  
Processing Properties Metric English Comments
Annealing Temperature 760 - 800 °C 1400 - 1470 °F Soft Annealing
(退火温度760-800)
  
化学成分:
Material Components Properties Metric English Comments
Carbon,    C   0.420 % 0.420 %  
Chromium,   Cr 13.0 % 13.0 %  
Iron,        Fe 86.58 % 86.58 %

评分

参与人数 1热处理币 +5 收起 理由
szchyuan + 5 鼓励鼓励!

查看全部评分

回复 顶 踩

使用道具 举报

签到天数: 3 天

[LV.2]偶尔看看I

 楼主| 发表于 2008-9-18 15:05:47 | 显示全部楼层
虽然不是很全,但是还是要谢谢你!
回复 顶 踩

使用道具 举报

签到天数: 971 天

[LV.10]以坛为家III

发表于 2008-10-18 11:22:07 | 显示全部楼层
原帖由 ych 于 2008-9-17 14:27 发表
2083是瑞士的一种不锈钢,用于注塑模具,如果你懂英文,可以到
www.matweb.com 查看。
Swiss Steel International THYROPLAST? 2083 Plastic Mold Steel  
Categories:  Metal; Ferrous Metal; Tool Steel; Mold Steel

...

2083好像是德国牌号吧?
回复 顶 踩

使用道具 举报

您需要登录后才可以回帖 登录 | 立即注册

本版积分规则

QQ|Archiver|手机版|小黑屋|热处理论坛 ( 苏ICP备2021037530号|苏公网安备32059002001695号 )
Copyright © 2005-2026, rclbbs.com 苏州热协网络技术有限公司 版权所有

GMT+8, 2026-10-28 15:13 , Processed in 0.023880 second(s), 22 queries .

Powered by Discuz! X3.5

© 2001-2026 Discuz! Team.

快速回复 返回顶部 返回列表