11055| 20
|
[求助] 3Cr13调质+高频未发现裂纹,但使用后出现裂纹,原因? |
| ||
| ||
| ||
| ||
| ||
| ||
| ||
| ||
| ||
| ||
| ||
| ||
| ||
点评
点赞!
| ||
| ||
| ||
| ||